  • Pozycja
    Granulation of Cu-Al-Fe-Ni Bronze
    (2014) Pisarek, Bogusław
    With the increase in wall thickness of the casting of iron-nickel-aluminium-bronze, by the reduction of the cooling rate the size of κII phase precipitates increases. This process, in the case of complex aluminium bronzes with additions of Cr, Mo and W is increased. Crystalliza-tion of big κII phase, during slow cooling of the casting, reduces the concentration of additives introduced to the bronze matrix and hard-ness. Undertaken research to develop technology of thick-walled products (g> 6 mm) of complex aluminium bronzes. Particular attention was paid to the metallurgy of granules. As a result, a large cooling speed of the alloy, and also high-speed solidification casting a light weight of the granules allows: to avoid micro-and macrosegregation, decreasing the particle size, increase the dispersion of phases in multiphase alloys. Depending on the size granules as possible is to provide finished products with a wall thickness greater than 6 mm by infiltration of liquid alloy of granules (composites). Preliminary studies was conducted using drip method granulate of CuAl10Fe5Ni5 bronze melted in a INDUTHERM-VC 500 D Vacuum Pressure Casting Machine. This bronze is a starting alloy for the preparation of the complex aluminium bronzes with additions of Cr, Mo, W and C or Si. Optimizations of granulation process was carried out. As the pro-cess control parameters taken a casting temperature t (°C) and the path h (mm) of free-fall of the metal droplets in the surrounding atmos-phere before it is intensively cooled in a container of water. The granulate was subjected to a sieve analysis. For the objective function was assume maximize of the product of Um*n, the percentage weight "Um" and the quantity of granules 'n' in the mesh fraction. The maxi-mum value of the ratio obtained for mesh fraction a sieve with a mesh aperture of 6.3 mm. In the intensively cooled granule of bronze was identified microstructure composed of phases: β and fine bainite (α+β'+β'1) and a small quantity of small precipitates κII phase. Get high microhardness bronze at the level of 323±27,9 HV0,1.
  • Pozycja
    Effect of Water Mist Cooling on Microstructure of Hypereutectic Al-Si Alloy
    (2014) Władysiak, Ryszard; Kozuń, Artur
    The work is a continuation of research on the use water mist cooling in order to increase efficiency of die-casting aluminum alloys using multipoint water mist cooling system. The paper presents results of investigation of crystallization process and microstructure of synthetic hypereutectic AlSi20 alloy. Casts were made in permanent mold cooled with water mist stream. The study was conducted for unmodified AlSi20 alloy and modified with phosphorus, titanium and boron on the research station allowing sequential multipoint cooling using a dedicated program of computer control. The study demonstrated that the use of mold cooled with water mist stream allows the formation of the microstructure of hypereutectic silumins. A wide range of solidification temperature of hypereutectic silumins increases the potential impact of changes in the cooling rate on a size, a number and a morphology of preeutectic silicon and eutectic α+β (Al+Si).