Tarbuk, AnitaČorak, IvanaĐorđević, DraganDraczyński, Zbigniew2022-11-242022-11-242022Tarbuk A., Čorak I., Đorđević D., Draczyński Z., Accelerated hydrolysis of PLA fibers at low temperature. W: AUTEX 2022 : 21st World Textile Conference AUTEX 2022 - AUTEX Conference Proceedings, Lodz University of Technology Press, Lodz 2022, s. 263-266, ISBN 978-83-66741-75-1, doi: 10.34658/9788366741751.55.978-83-66741-75-1http://hdl.handle.net/11652/4488https://doi.org/10.34658/9788366741751.55The polylactide (PLA) is the most common biodegradable material. However, its biodegradation requires hydrolysis of PLA to oligomers or monomers before microbes can act. Hydrolytic degradation of PLA depends on temperature, time and relative humidity. It takes months and years until complete biodegradation. If a catalyst is introduced, i.e. alkali or alcohol, it can be done in weeks. In this article, the alkaline hydrolysis was performed at low temperatures 40-60°C without and with the addition of cationic compound as an accelerator for the purpose of saving energy and time for complete PLA degradation. It has been shown that complete degradation can be achieved in only 10 min at 40°C.enDla wszystkich w zakresie dozwolonego użytkuFair use conditionPLAalkaline hydrolysiscationic surfactantlow temperaturehydroliza alkalicznakationowy środek powierzchniowo czynnyniska temperaturaAccelerated hydrolysis of PLA fibers at low temperatureartykuł - konferencjaLicencja PŁLUT License10.34658/9788366741751.55